We have the catalog including different kinds of standard bucket tooth specification,Side Pin Teeth And Adapter For CAT J200, J225, J250, J300, J400, J450/460, J550, J600, J700, J800 Teeth And Adapter For CAT Side Dump Bucket Unitooth For CAT 20, 25, 30, 35 Ripper Teeth For CAT R300, R350, R450, R500, R550 Ripper Guards And Ripper Shanks For CAT Grader Shanks And Teeth For CAT Weld-on Heel Shrouds For CAT, Side Bar Protectors For CAT Side Pin Teeth And Adapter For KOM PC60PC1250 Unitooth For KOM WA30WA600, Ripper Teeth For KOM Conical Teeth And Adapter For ESCO 18, 22, 25, 30, 35, 40, 45, 50, 55 Super Conical Teeth And Adapter For ESCO: 36, 46, 56, 66, 76, 86 Helilok teeth And Adapter For ESCO: 21, 27, 37, 47, 57 Ripper Teeth For ESCO: 22, 25, 35, 39 Teeth And Adapter For H amp L: 23, 24 Teeth For HENSLEY: 156, 220, 290, 310, 330, 370, 400, 410, 550 Teeth And Adapter For Volvo Teeth And Adapter For BOFORS B0, B1, B2, B3, B4 Teeth And Adapter For FIAT 22, 24, 26, 28 Teeth amp Adapter For BOBCAT, Unitooth For HMK Teeth For LIEBHERR, Teeth And Adapter For HYUNDAI V Series Teeth And Adapter For DAEWOO, Side Pin Ned Teeth And Adapter For DAEWOO Teeth For KOBELCO, Unitooth For KAWASAKI MINI Unitooth, FAI Kom (FMK) FK Unitooth For FIAT Hitachi FIAT New Holland, Unitooth For JCB Teeth And Adapter For Hitachi, Teeth And Adapter For Case. |
|
|
|
|
Process Description |
Investment Casting There are three techniques in our investment casting process including water glass technique casting, silica sol technique casting and lost foam casting. Water glass technique casting Water glass technique casting is also called cryogenic lost wax. And the dimension tolerance we could reach is CT7-8.The main material is carbon steel, alloy steel. The weight controlled is about 0.2-80 kg. Silica sol technique casting Silica sol technique casting is also called mesothermal lost wax. And the dimension tolerance we could reach is CT5-6.The main material is stainless steel ,carbon steel, alloy steel. The weight controlled is about 0.1-60kg. Lost foam casting Lost foam casting is a modern form of investment casting that eliminates certain steps in the process. And the dimension tolerance we could reach is CT8-9.The main material is gray iron, dutile iron, high Cr cast iron, resistance cast iron. The weight controlled is about 0.2-100 kg. |
Investment casting process |
|
|
1. Mould Designing
Strictly making 3D model based on customer’s drawing dimensions, and mastered the contractibility rate for all types of material. |
2. Wax Injection Wax design of the desired castings are produced by injection molding. These
designs are called patterns. |
|
|
3. Assembly The patterns are attached to a central wax stick, called a sprue, to form a casting cluster or assembly. |
4. Shell Building The shell is built by immersing the assembly in a liquid ceramic slurry and then into
a bed of extremely fine sand. Up to eight layers may be applied in this manner. |
|
|
5. Dewax At this point, all of the residual pattern and gating material is removed, and the ceramic mold remains. The mold is then preheated to a specific temperature and filled with molten metal, creating the metal casting |
6. Mould Shell Roast:
This process is to put the lost-wax shell into the roast furnace and make them harder. Heating the Mould shell before casting is also to ensure the better products surface texture. |
|
|
7. Smelting the Liquid Steel:
Allocate the chemical composition and sampling before steel casting. |
8.Spectrochemistry Analysis Inspection on materials by spectrometer testing. |
|
|
9. Conventional Casting In the conventional process, the shell is filled with molten metal by gravity pouring. |
10. Cut Off The parts are cut away from the central sprue using a high speed friction saw. |
|
|
11.Heat Treating
Carbon steel and low-alloy steel need normalizing and temper, oil-quenching, water-quenching and so on. We can set out different heat treatment method as per different requirement from customers. |
12. Polishing Polishing is to modify the out of flatness on casting head after casting cuttig and to modify the burring and splashings in the process of casting cycle. |
|
|
13. Inspection:
Inspection of the mechanical properties, surface, internal quality, and to check if the rough dimension meet the drawing requirement for the prodcuts. |
14. Machining
Cut the piece of raw material into a desired final shape and size. Now we have CNC, Lathe, milling machine, drilling machine, boring lathe and grinding machine. |
|
|
15.Quality Inspection: Quality inspection on the machining dimension. Mainly tools we use is like specialized gauge and callipers, mircocalliper,three-dimensional and so on. |
16. Storage and Delivery
Efficiency of package goods delivery on time per your shipping requests. |
Advantage of investment casting |
Wide Application Scope Our investment casting process is virtually unrestricted by the size ,thickness and shape complexity. Wide Choice of Alloys Our investment casting process able to utilize a wide variety of alloys for common carbon steel, alloy steel, manganese steel,stainless steel ,and high-Cr & wear-resist Iron and so on. Dimensional accuracy The investment casting process is capable of producing foundry with higher accuracy than ordinary forgings and weld assembly in general condition. Reduction of Production Costs Investment castings are able to reduce costs in many cases such as reduced machining, less materiel waste and so on. |
In addition, we own CNC machining center and CNC Lathe, so machine parts (machining parts or machinery parts),metalwork (metal products) are ok for us! |
| |
|
|
|
|